XGD® 60

Technical specification

Thermal  
Temperature resistance (short-term)250 °C482 °F
Temperature resistance (long-term)210 °C410 °F
Thermal conductivity0.3 W/mK0.17 btu/ft h °F
Coefficient of linear expansion12·10-612·10-6
Mechanical    
Compressive strength (room temperature) 610 N/mm2 88473 psi
Flexural strength 500 N/mm2 72518 psi
Compressive strength (200°C)300 N/mm2 43511.3 psi